We could produce VASCOMAX C250 springs,VASCOMAX C-250 springs,VASCOMAX C-250 Compression Springs,VASCOMAX C250 Extension Springs,VASCOMAX C250 Torsion Springs,VASCOMAX C-250 tension spring, VASCOMAX C250 disc spring, VASCOMAX C250 wave spring,VASCOMAX C-250 Spiral Springs,VASCOMAX C250 Automotive Springs,VASCOMAX C250 Elevator Springs,VASCOMAX C250 coil springs,VASCOMAX C250 Conical Springs,VASCOMAX C250 Tapered Springs,VASCOMAX C250 Barrel Springs,VASCOMAX C-250 die springs,VASCOMAX C-250 Constant Force Springs,VASCOMAX C-250 Power Springs,VASCOMAX C-250 Garter Springs,VASCOMAX C250 retaining Springs,VASCOMAX C250 Volute Springs,VASCOMAX C250 flat springs,VASCOMAX C250 Volute Springs,VASCOMAX C250 battery springs,VASCOMAX C250 Spring Clips,VASCOMAX C250 Battery Contacts from china

The diameter of VASCOMAX C250 springs that we could do range from 0.30 mm to 3.00 mm.

As per Surface finish of VASCOMAX C250 springs, we could do grinding ,presetting ,deburring ,shot peening ,vibratory finishing ,passivating,painting ,heat setting,stress relief ,end forming,threading ,coining,chamfering ,knurling ,welding ,assembly,grooving ,flatting and so on

As per Coatings of of VASCOMAX C250 springs, we could do chrome,Teflon, corvel,pain,color coding,zinc plating,black oxide,precoated wire and so on

Our VASCOMAX C250 Springs could undergo either bainitic hardening after forming (carbon) or vacuum hardening and annealing (stainless).or come in pre-hardened As per the requirement of the clients

VASCOMAX C250  combines ultra-high strength (1800MPa), good toughness, readily machinable in pre-aged condition, excellent transverse properties and resistance to crack propagation


The chemical composition of VASCOMAX C-250 springs is as follows

Table 1. Chemical composition of VascomaxC250

Chemical Elements

Min

Max

Nickel

17.0

19.0

Molybdenum

4.6

5.1

Cobalt

7.0

8.5

Carbon

-

0.03

Aluminum

0.05

0.15

Phosphorus

-

0.01

Sulfur

-

0.01

Silicon

-

0.10

Titanium

0.3

0.5

Manganese

-

0.01

Iron

68.0

-


The mechanical property of VASCOMAX C250 spring is as follows

Table 2. Mechanical properties forsolution annealed maraging alloy 250

816°C (1500°F), 1hr, AC

Metric

English

Tensile Strength, Ultimate

1000 MPa

145 ksi

Tensile Strength, Yield

793 MPa

115 ksi

Percent Elongation

20%


We could do solution treatment and ageing treatment for VASCOMAX C250 springs as per the requirement of the clients.

We could supply inspection certificate of VASCOMAX C250 springs by third party,like TUV,DNV,GL,BV,SGS and so on

We analyze your VASCOMAX C250 spring design and make recommendations to improve quality and reduce cost. Whether you have a sample, drawing or idea, our engineering team is ready to offer you design assistance and material recommendation to best fit your application as well as your budget. We are easy to talk to, well-prepared and ready to put our expertise to work for you.

Our VASCOMAX C-250 springs are widely used in chemical pump,plunger pumps,Cement Mill ,sugar Mill,concrete mills and mixers,processing units,mechanical equipment, crystalizer equipment,Wellhead and Christmas tree,power transmission, turbine,gas compressor,gear boxes and so on.