We are professional ASTM A336 F9 ASTM A182-F9 ASME SA182 F9 ASME Sa 336 SA336 F9 P9 T9 Grade F9 forged forging rings seamless rolled rings forged forging Sleeves Bushes Bushing Pipes Piping tube tubings barrels Casing Cases Shells blocks round bars hollow bars cylinders hubs housings,ASTM A336 F9 ASTM A182-F9 ASME SA182 F9 ASME Sa 336 SA336 F9 forged forging steel discs disks tubesheets tube sheets tube plates,ASTM A336 F9 ASTM A182-F9 ASME SA182 F9 ASME Sa 336 SA336 F9 forged forging steel valve body bodies blocks valve bonnets valve stems valve closures valve seat rings valve parts valve components,ASTM A336 F9 ASTM A182-F9 ASME SA182 F9 ASME Sa 336 SA336 F9 forged forging steel Girth flange Channel cover shafts forged forging FVC type Self Reinforced Nozzle Long welding neck Nozzle neck Flanges Cover Flanges,Shell Tube Heat Exchanger components parts forged forging pieces forged forging steel components ASTM A336 F9 ASTM A182-F9 ASME SA182 F9 ASME Sa 336 SA336 F9 FRONT REAR Fixed STATIONARY Floating Cladding Clad Cladded Welding Welded Overlay Overlayed Coated Tube Sheets TUBESHEET from china
ASTM A336 F9 ASTM A182-F9 ASME SA182 F9 ASME Sa 336 SA336 F9 P9 T9 Grade F9 Chemical Compositions(%)
Compositions | Data |
UNS Designa-tion | |
Carbon(max.) | 0.15 |
Manganese | 0.30-0.60 |
Phosphorus(max.) | 0.025 |
Silicon(max.) | 0.50 |
Chromium | 4.00-6.00 |
Molybdenum | 0.45-0.65 |
Other Elements | … |
Temperature T °C/F (°C/F) | Specific heat J / kgK (Btu / lb °F) | Thermal conductivity W/mK (Btu·in / ft2·h·°F) | Electric resistance µΩ · cm (Ω circ mill / ft) | Modulus of elasticity kN/mm2 (103 ksi) | Expansion rate from 70°F bis T 10-6 / K (10-6 / °F) |
---|---|---|---|---|---|
20/ | 21/() | 217 | |||
100/ | 23/() | ||||
200/ | 24/() | ||||
300/ | 26/() | ||||
400/ | 27/() | ||||
500/ | 28/() | ||||
600/ | 29/() |
Temp. | Creep strain limit | Creep strain limit | Creep rupture strength | Creep rupture strength | Creep rupture strength |
---|---|---|---|---|---|
°C/°F | 100 000 h | 200 000H | |||
°C/°F | Mpa / ksi | Mpa /ksi | |||
400 / 752 | |||||
450 / 842 | 276 / 40,0 | 259 / 37,5 | |||
480 / 896 | 211 / 30,6 | 196 / 28,4 | |||
500 / 932 | 174 / 25,2 | 160 /23,2 | |||
550 / 1022 | 92 / 13,3 | 80 / 11,6 | |||
ksi value calculated |
Mechanical properties (20°C / 68°F)
yield strenght Rp 0,2 N/mm2 /ksi | 220-390 /31,9-56,5 | ||
---|---|---|---|
tensile strenght Rm(N/mm2) /ksi | 590-750 /85,5-108,7 | ||
Elongation (lengthwise/transverse) (%) | 20 % /18 % | ||
impact work (ISO-V- Charpy-V | > 40J | lengthwise |
Temparature information
Application area | ||
---|---|---|
Operation temperature | 14 ºF to 1022 ºF |
hardness | ||
---|---|---|
Working temperature | 1634 ºF to 1742 ºF | |
Explanation report | cooldown: air/oil |
Solution heat treatment | ||
---|---|---|
Working temperature | 1472 ºF to 2012 ºF |
annealing | ||
---|---|---|
Working temperature | 1328 ºF to 1472 ºF | |
Explanation report | cooldown: air |
Normalizing | ||
---|---|---|
Working temperature | 1634 ºF to 1742 ºF |
Heat treating | ||
---|---|---|
Working temperature | 1562 ºF to 2012 ºF |
-
New
·1.4898 Bars ·1.4886 Bars ·1.4529 Bars ·1.4876 Bars ·2.4856 Bars ·2.4851 Bars ·2.4816 Bars ·2.4668 Bars ·2.4663 Bars ·2.4642 Bars -
Any
·UNS N09979 Bars ·Incoloy 890 Bars ·UNS S34800 Bars ·Inconel 686 Bars ·UNS N13017 Bars ·Inconel 600 Bars ·UNS N06002 Bars ·UNS N10675 Bars ·UNS N06200 Bars ·UNS N06025 Bars -
Hot
·Inconel 600 Bars ·Inconel 601 Bars ·Inconel 617 Bars ·Inconel 625 Bars ·Inconel 686 Bars ·Inconel 690 Bars ·Inconel 693 Bars ·Inconel 718 Bars ·Inconel 725 Bars ·Inconel 751 Bars